Brand Name: | Yuhong |
Model Number: | ASTM A312, TP347H |
MOQ: | 100KGS |
Packaging Details: | Ply-wooden Case /Iron Case/ Bundle with plastic Cap |
Payment Terms: | L/C, T/T |
Material | TP347H |
Fin Material | Stainless Steel |
Fin Thickness | 1.54mm |
Base Tube Test | HT, ET |
Fin Tube Test | Size Inspection |
Application | HRSG system |
High-Frequency Welding (HFW) finned pipes made from ASTM A312 TP347H stainless steel are specifically designed for Heat Recovery Steam Generators (HRSG). HRSG systems are critical components in combined-cycle power plants, capturing waste heat from exhaust gases to generate steam for energy efficiency. The use of TP347H stainless steel ensures excellent resistance to high temperatures, corrosion, and oxidation.
Element | Content (%) |
---|---|
Carbon (C) | ≤ 0.04% |
Manganese (Mn) | 1.00 - 2.00% |
Phosphorus (P) | ≤ 0.045% |
Sulfur (S) | ≤ 0.030% |
Silicon (Si) | ≤ 0.75% |
Chromium (Cr) | 17.00 - 19.00% |
Nickel (Ni) | 9.00 - 13.00% |
Molybdenum (Mo) | ≤ 0.30% |
Niobium (Nb) | 1.00 - 1.50% |
Property | Value |
---|---|
Tensile Strength | ≥ 515 MPa |
Yield Strength | ≥ 205 MPa |
Elongation | ≥ 40% |
Impact Energy | ≥ 70 J (at -196°C) |
Hardness | ≤ 170 HB |
Proof Stress | ≥ 205 MPa |
Brand Name: | Yuhong |
Model Number: | ASTM A312, TP347H |
MOQ: | 100KGS |
Packaging Details: | Ply-wooden Case /Iron Case/ Bundle with plastic Cap |
Payment Terms: | L/C, T/T |
Material | TP347H |
Fin Material | Stainless Steel |
Fin Thickness | 1.54mm |
Base Tube Test | HT, ET |
Fin Tube Test | Size Inspection |
Application | HRSG system |
High-Frequency Welding (HFW) finned pipes made from ASTM A312 TP347H stainless steel are specifically designed for Heat Recovery Steam Generators (HRSG). HRSG systems are critical components in combined-cycle power plants, capturing waste heat from exhaust gases to generate steam for energy efficiency. The use of TP347H stainless steel ensures excellent resistance to high temperatures, corrosion, and oxidation.
Element | Content (%) |
---|---|
Carbon (C) | ≤ 0.04% |
Manganese (Mn) | 1.00 - 2.00% |
Phosphorus (P) | ≤ 0.045% |
Sulfur (S) | ≤ 0.030% |
Silicon (Si) | ≤ 0.75% |
Chromium (Cr) | 17.00 - 19.00% |
Nickel (Ni) | 9.00 - 13.00% |
Molybdenum (Mo) | ≤ 0.30% |
Niobium (Nb) | 1.00 - 1.50% |
Property | Value |
---|---|
Tensile Strength | ≥ 515 MPa |
Yield Strength | ≥ 205 MPa |
Elongation | ≥ 40% |
Impact Energy | ≥ 70 J (at -196°C) |
Hardness | ≤ 170 HB |